– Creamic MgO・Al2O3・SiO2 is formed by cordierite crystal 2MgO・2Al2O3・5SiO2. This material has two type, we called it N-23 and N-53.
-Especially, N-53 has more Nishimura’s originality. N-53 has a self-gazed wonderful appearance.
Feature
-High thermal shock resistance
-Low thermal expansion
Application
-Thermal resistance parts (Air heater, Heater parts)
-low thermal expansion required parts
Information
Information |
||
Nishimura No. | N-23 | N-53 |
Main component | 2MgO・2Al2O3・5SiO2 | 2MgO・2Al2O3・5SiO2 |
Bulk specific gravity | 2.2 | 2.7 |
Water absorption | <0.5% | 0% |
Bending strength | 120MPa | 120MPa |
Dielectric constant | 4(1MHz) | 4(1MHz) |
Dielectric loss tangent | 4.0×10-4(1MHz) | 5.0×10-4(1MHz) |
Thermal expansion coefficient | 2.8×10-6/℃ | 2.6×10-6/℃ |
Thermal conductivity | 1.25W/mK | 2.5W/mK |
Thermal shock resistance | 400℃ | 150℃ |