This material is toughened by adding zirconia, which has high wear resistance and high fracture toughness, to hard and high thermal conductivity alumina.
15% zirconia and 30%. zirconia are available to suit your needs.
Feature
High thermal conductivity and High wear resistance by combining zirconia and alumina.
| Nishimura No. | N-AZ15 | N-AZ30 |
| Amount of zirconia added | 15% | 30% |
| specific gravity (g/cm3) | 4.2 | 4.4 |
| bending strength (Mpa) | 610 | 600 |